I've heard lots on my time Lee. The only reasons that resonated with me were:
1. To overcome moisture uptake of the boards between cleaning and coating if significant delay between 2 processes. High levels of moisture can create havoc with certain solvent-based materials developing their adhesion, or lead to blushing, where coating becomes cloudy, hazy or milky in appearance. Can lead to bubbling with moisture curing mechanisms occurring at a rate greater than the permeation of by products, eg CO2 thru the film.
2. To help prevent excessive capillary flow or dripping on inversion with low viscosity solvent-based materials, theory being drive solvent-off quicker, build viscosity faster. This works well with primer or 'dusting' layers, less well with traditional cc process.
I don't see this 2nd reason cited much any more. Sure I missed some reasons though...
Best Regards,
Phil
+44 7703 795422
Sent from my iPhone
On 26 Mar 2013, at 17:39, lee Hitchens <[log in to unmask]> wrote:
> Can I also ask a question. What is the purpose of baking a PCB before
> coating, assuming that the cleaning process drying section is adequate? I
> have never really got a good answer to this?
>
> Best Regards
>
> Lee Hitchens
> Technical Director
>
> SCH Technologies is a Division of SCH Services Limited
> Mob: +44 (0) 7862 25 33 21 www.conformalcoating.co.uk
>
> TECHNICAL SUPPORT SERVICE
>
> SCH Services Ltd offers a Technical Support Helpline to help address all
> issues relating to reliability. This includes contamination testing,
> cleanliness and cleaning issues, plus any coating related questions.
> Please contact us via email or telephone:
>
> [log in to unmask] +44 (0)1226 249019 (office hours & answerphone) +44
> (0)7862 253321 (out-of-hours emergency)
>
> The opinions expressed in this e-mail are strictly those of the sender and
> not of SCH Services Limited. This communication may contain information
> which is confidential and may also be privileged. It is for the exclusive
> use of the intended recipient(s). Unauthorised use, copying or disclosure of
> any of it may be unlawful. If you are not the intended recipient(s) please
> note that any distribution, copying or use of this communication or the
> information in it is strictly prohibited. If you have received this
> communication in error please notify us by e-mail or by telephone (+44
> (0)1226 249019) and then delete the e-mail and any copies of it. Virus
> Warning - Although steps have been taken to ensure that all email and
> attachments are virus-free, we cannot guarantee nor be held liable.
>
> Company Registration: 04043334
> Registered office: SCH Services Limited Newburgh Building McLintock Way
> Barnsley South Yorkshire S70 6BF
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Fox, Ian
> Sent: 26 March 2013 16:17
> To: [log in to unmask]
> Subject: Re: [TN] Conformal Coat and Board Edges
>
> No we don't. Since the purpose of the coating is not to prevent moisture
> ingress into the board (we all know that happens), but really to prevent
> issues with condensation, and since there likely will be no exposed tracks
> on the edge, there's no point. We typically have a ground/thermal strip
> around the edge of the card anyway so the masking may sometimes cover, or
> partially cover the edge. I couldn't tell you how many millions of on wing
> hours our assemblies have accumulated over the past 30+ years, but we've
> never had an issue in service as a result of uncoated edges, nor in the
> umpteen unit qualifications we've carried out. In fact if you carry out
> weight gain measurements with high (85%+) humidity exposure the laminate is
> typically saturated after about 4 days and we always run the 10 day tropical
> exposure test
>
> Regards
>
> Ian Fox
> Lead Materials and process Engineer
>
> Aero Engine Controls
> York Road, Hall Green, Birmingham B28 8LN | Tel: +44 (0)121 607 3763 | Fax:
> +44 (0)121 607 3975
> Email: [log in to unmask] | Web: www.aeroenginecontrols.com
>
> Aero Engine Controls is part of the Rolls-Royce Group
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
> Sent: 26 March 2013 15:43
> To: [log in to unmask]
> Subject: [TN] Conformal Coat and Board Edges
>
> OK, the conformal coat question of the day:
>
> Do you conformally coat the edges of a printed circuit assembly? Why or why
> not?
>
> OK, that is two questions, or perhaps a half fractional question.....
>
> Doug Pauls
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned.
>
> ______________________________________________________________________
> Aero Engine Controls is part of the Rolls-Royce Group, whose legal entity is
> Rolls-Royce Engine Control Systems Limited which is registered in England.
> Registered office at Moor Lane, PO Box 31, Derby, DE24 8BJ. Company number
> 6686268, UK VAT number GB 939 396 075
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|