I have never seen an inline cleaner that could completely remove all of the entrapped moisture from a populated CCA. Unless the CCA is actually baked in an oven for a minimum of 45 minutes at 105 deg. C, you will have entrapped moisture inside connector pins, underneath larger SMT packages as well as BGAs, etc. This can cause issues both during testing and will prevent good adhesion of CC. The CCA needs to be both clean and dry.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of lee Hitchens
Sent: Tuesday, March 26, 2013 11:40 AM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coat and Board Edges
Can I also ask a question. What is the purpose of baking a PCB before coating, assuming that the cleaning process drying section is adequate? I have never really got a good answer to this?
Best Regards
Lee Hitchens
Technical Director
SCH Technologies is a Division of SCH Services Limited
Mob: +44 (0) 7862 25 33 21 www.conformalcoating.co.uk
TECHNICAL SUPPORT SERVICE
SCH Services Ltd offers a Technical Support Helpline to help address all issues relating to reliability. This includes contamination testing, cleanliness and cleaning issues, plus any coating related questions.
Please contact us via email or telephone:
[log in to unmask] +44 (0)1226 249019 (office hours & answerphone) +44
(0)7862 253321 (out-of-hours emergency)
The opinions expressed in this e-mail are strictly those of the sender and not of SCH Services Limited. This communication may contain information which is confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). Unauthorised use, copying or disclosure of any of it may be unlawful. If you are not the intended recipient(s) please note that any distribution, copying or use of this communication or the information in it is strictly prohibited. If you have received this communication in error please notify us by e-mail or by telephone (+44
(0)1226 249019) and then delete the e-mail and any copies of it. Virus Warning - Although steps have been taken to ensure that all email and attachments are virus-free, we cannot guarantee nor be held liable.
Company Registration: 04043334
Registered office: SCH Services Limited Newburgh Building McLintock Way Barnsley South Yorkshire S70 6BF
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fox, Ian
Sent: 26 March 2013 16:17
To: [log in to unmask]
Subject: Re: [TN] Conformal Coat and Board Edges
No we don't. Since the purpose of the coating is not to prevent moisture ingress into the board (we all know that happens), but really to prevent issues with condensation, and since there likely will be no exposed tracks on the edge, there's no point. We typically have a ground/thermal strip around the edge of the card anyway so the masking may sometimes cover, or partially cover the edge. I couldn't tell you how many millions of on wing hours our assemblies have accumulated over the past 30+ years, but we've never had an issue in service as a result of uncoated edges, nor in the umpteen unit qualifications we've carried out. In fact if you carry out weight gain measurements with high (85%+) humidity exposure the laminate is typically saturated after about 4 days and we always run the 10 day tropical exposure test
Regards
Ian Fox
Lead Materials and process Engineer
Aero Engine Controls
York Road, Hall Green, Birmingham B28 8LN | Tel: +44 (0)121 607 3763 | Fax:
+44 (0)121 607 3975
Email: [log in to unmask] | Web: www.aeroenginecontrols.com
Aero Engine Controls is part of the Rolls-Royce Group
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: 26 March 2013 15:43
To: [log in to unmask]
Subject: [TN] Conformal Coat and Board Edges
OK, the conformal coat question of the day:
Do you conformally coat the edges of a printed circuit assembly? Why or why not?
OK, that is two questions, or perhaps a half fractional question.....
Doug Pauls
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned.
______________________________________________________________________
Aero Engine Controls is part of the Rolls-Royce Group, whose legal entity is Rolls-Royce Engine Control Systems Limited which is registered in England.
Registered office at Moor Lane, PO Box 31, Derby, DE24 8BJ. Company number 6686268, UK VAT number GB 939 396 075
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|