TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 6 Mar 2013 09:58:18 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lloyd Duso <[log in to unmask]>
Message-ID:
Subject:
From:
Lloyd Duso <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (104 lines)
Exactly. There is no reason to use anything too aggressive with 1B31.
Acrylics are very weak solvent wise. Now if it was fully cured UR, that's a
different story.

Lloyd E Duso
Diamond-MT
Plant Manager
(814) 535-3505
 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, March 06, 2013 9:05 AM
To: [log in to unmask]
Subject: Re: [TN] Coating stripping facility

While I agree with Patrick that this stuff works, it is Tetrahydrofuran, a
nasty material and very aggressive.  And if you have the possibility of
operators mixing soldering irons with THF, you get some frightening
breakdown products.  We used to use these, but got away from it completely.

Straight toluene or xylene will strip 1B31 pretty effectively and is much
less costly or hazardous than THF, especially if you are doing a few hundred
assemblies.  And you have some good recommendations for companies that will
do this for you.

Doug Pauls



From:   "Goodyear, Patrick" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   03/06/2013 07:00 AM
Subject:        Re: [TN] Coating stripping facility
Sent by:        TechNet <[log in to unmask]>



Ioan, 

When we need to remove conformal coatings for repairs we use Conformal
Coating Remover from Trace Technologies, we get it from TechSpray in
Amarillo Texas 806-3728523  www.techspray.com
MSDS (Material Safety Data Sheets) can be found online.    Very effective 
for removing HumiSeal and others. 
We have it in 1Qt. Bulk and in 12.5ml pens, great for spot application. 

Pat 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Tuesday, March 05, 2013 12:19 PM
To: [log in to unmask]
Subject: [TN] Coating stripping facility

Dear Technos,

I'm looking for a facility able to strip 1B31 from a few hundreds of boards
preferably in Eastern Canada or US New England. On or offline answers
appreciated, no sub contractor is a priori disqualified, even if in CA.

Thanks,

Ioan Tempea, ing.
Ingénieur principal de fabrication / Senior Manufacturing Engineer
[signature002]<http://www.digico.cc/>

950 RUE BERGAR, LAVAL, QC, H7L 5A1<http://g.co/maps/2gh3f>
T+ 1 (450) 967-7100, EXT244
------------------------------------------------------------------------
  [signature001] <http://www.facebook.com/pages/Digico/277076778479>
------------------------------------------------------------------------
Lauréat Dunamis 2012<http://digico.cc/dunamis-2012/>
Entreprise manufacturière / Gestion du capital humain


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


PG&E is committed to protecting our customers' privacy. 
To learn more, please visit 
http://www.pge.com/about/company/privacy/customer/

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2