Technetters, I am looking at some printed circuit boards with ENIG finish, which have a requirement that they pass J-STD-003B, class 3, solderability testing, with durability 3 conditioning (72% humidity at 85 C for 8 hours).
IPC-4552, Appendix 3, 'Qualification of ENIG process' says 'Solderability shall meeting requirements of J-STD-003 Category 3...'
Looking at the draft J-STD-003C, Table 1-3, lists ENIG among numerous surface finishes requires solderability acceptable after exposure to default conditioning parameters corresponding to durability 3.
Is conformance by ENIG to such a requirement achievable in reality?
Louis Hart
Compunetics
Monroeville, PA
USA
[log in to unmask]<mailto:[log in to unmask]>
412-858-1232
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|