TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Richard Kraszewski <[log in to unmask]>
Date:
Fri, 22 Mar 2013 08:19:04 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Douglas Pauls <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Rich Rich Rich,
You are supposed to answer all the hard questions for me so I don't have 
to work so hard <grin>.

Let me ask the question another way.  Plexus, being a high quality 
reputable EMS company, has acceptability standards on conformal coating 
film quality, both your own and imposed upon you by your customers.  Do 
your customers ever differentiate conditions where bubbles are acceptable? 
 Or are they all - here are our specifications, but we have no idea where 
they come from or their basis in reality?  I can't really point fingers in 
this case.  Our own internal standards say that a bubble cannot be greater 
than 90 mil diameter, or a cluster of bubbles cannot be greater than 90 
mils.  Been that way for decades and damned if I can find any technical 
studies here upon which that figure was founded.

The more I work on this, the more I realize that bubbles in coating are 
something that is hard to quantify, but "I know it when I see it" kinda 
thing.

And for #3, would you lump together all liquid coatings in terms of 
bubbles, irregardless of coating chemistry, and make a separate set of 
criteria for vapor deposited coatings such as Parylene?

Doug Pauls



From:   Richard Kraszewski <[log in to unmask]>
To:     TechNet E-Mail Forum <[log in to unmask]>, 
"[log in to unmask]" <[log in to unmask]>
Date:   03/21/2013 10:47 PM
Subject:        RE: [TN] Conformal Coat and Bubbles



#1 Yes allowed. AABUS(sorry- yes I know, not much help here). 
#2  I have  seen reference to a defense sector customer spec referencing a 
bubble defined as being an issue if greater than or equal to 1/16 of an 
inch. No supporting data for this.
#3  No, if for no other reason than FOD.

Rich Kraszewski
(920)969-6075
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Thursday, March 21, 2013 9:19 AM
To: [log in to unmask]
Subject: [TN] Conformal Coat and Bubbles

OK, Minions, your next question in the quest to improve J-STD-001 and 
A-610 relates to bubbles in the conformal coating.

I think we can all agree that the ideal conformal coating layer contains 
no bubbles or voids and is "purdy".    BUT:

1.  Are there bubbles in coatings in areas where they will not impact 
reliability and their presence should be viewed as a "Process Indicator"? 
If so, where and what limits would you use?

2.  What would you classify as a bubble requiring disposition, i.e. 
Becomes an actionable defect?  If so, where and why?

3.  Would any of your answers change depending on what KIND of coating it 
is, i.e. Acrylic vs. silicone vs. Parylene?

Well, OK, that is three questions.  I'm on a roll.


Doug Pauls
Chairman, IPC Cleaning and Coating Committees
Galactic Emporer



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2