TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Joyce Koo <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 21 Mar 2013 18:04:09 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Glidden, Kevin" <[log in to unmask]>
Message-ID:
Subject:
From:
"Glidden, Kevin" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (60 lines)
Are you implying they are higher or lower?????

I was just guessing and giving a "for instance"... I don't really know what Class (if any) they claim to be built to.


Kevin Glidden


-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]] 
Sent: Thursday, March 21, 2013 2:00 PM
To: 'TechNet E-Mail Forum'; Glidden, Kevin
Subject: RE: [TN] Explaining why pretty solder joints arn't good solder joints

Wow.  X-box is class 1?  

Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Thursday, March 21, 2013 1:51 PM
To: [log in to unmask]
Subject: Re: [TN] Explaining why pretty solder joints arn't good solder joints

Because a whole BUNCH of REALLY smart people sat in a room for MANY MANY hours at a time over many years to develop and document acceptable solder joint inspection criteria, based on real world experiences and testing.  That document is called IPC-A-610.  And it, my friends, says thou shalt not have ANY end overhang of a chip component (ref IPC-A-610E section 8.3.2.2).  This is for even Class 1 product (Teddy Ruxpin's and Xbox's).   And, btw, a partial listing of that group of super-smart people is listed right at the front of the document, from all sorts of industry leading, highly successful companies.

Just my 2 cents.

What are the contractual obligations for acceptance criteria?

Another option is to turn the tables.  IPC-610 brings evidence this is NOT acceptable.  Make them PROVE it if they think it is.


-----Original Message-----
From: Pete [mailto:[log in to unmask]]
Sent: Thursday, March 21, 2013 9:41 AM
To: [log in to unmask]
Subject: [TN] Explaining why pretty solder joints arn't good solder joints

We have a product on which the assembly vendor decided to change the power inductor we specified.  The part they used is close to the same size, but even at nominal, the leads overhand the pads on 3 sides under the body.  I raised a concern that these stress points create a risky solder joint.  The engineering group running this project keeps sending me pictures:  "look - it fits on the board and they got solder on the outside of the leads!"  I pointed out that the 3 sides of the joint they can't see are stress points.  Any tips on explaining the risk here?

Pete

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2