TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Tue, 19 Mar 2013 11:59:04 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Larry Dzaugis <[log in to unmask]>
Subject:
From:
Larry Dzaugis <[log in to unmask]>
Message-ID:
In-Reply-To:
<76D05A7634B94E838431A2FD9684F363@stephenPC>
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (19 lines)
It is in the manual, which they should have or can request a soft copy from
Vitronic Soltec.
The service desk has the information.
Recommend using nuggets to recharge pot initially, 200 pounds.
One ton initial purchase total, bar and nuggets should do it and keep you
supplied for initial runs.

Highly recommend checking out the machine when it is empty.
Check out what alterations have been made in the control section.
VS does make changes and it is best to find out now which modules are
obsolete.
Lead free eats up machines such as the back gate and impellers.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2