Hi All,
I just got an email back from a guy named Derrick Herron of Indium who sent
me a really useful spreadsheet that makes it simple to calculate what you
need to take out of your pot, and how much tin you should add based on the
numbers you get back from an analysis to put everything back into spec, and
I thought that I would share this with everyone. Makes it dead simple even
for me!
http://stevezeva.homestead.com/Solder_Pot_Analysis.xlsx
Steve