TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Goodyear, Patrick" <[log in to unmask]>
Date:
Fri, 8 Mar 2013 19:37:24 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Afri Singh <[log in to unmask]>
Message-ID:
Subject:
From:
Afri Singh <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (63 lines)
There are some recyclers who will take pick it up and recycle it

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Monday, March 04, 2013 12:33 AM
To: [log in to unmask]
Subject: Re: [TN] BARE PCB disposing

Hmmm, well one could cut them into small chunks and make jewelry out of
them, ear rings and such.   Another possibility is to coat them in a
clear smooth finish and make clipboards out of them.   Depending on
traces etc. offer them up for soldering practice boards, test sample
processing, check with PACE worldwide or Circuit Medic to see if they
want them for practice kits.   If they are clean i.e. non-etched but
drilled boards offer them to the amateur radio community for
experimental board, especially if they have ground planes.   The metals
could be chemically removed and recycled.    I have actually obtained
rejected drilled copper plated double side boards that I mill the traces
on for building projects.    

Just a few ideas.   
Pat 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ramakrishnan
Saravanan
Sent: Friday, March 01, 2013 4:34 AM
To: [log in to unmask]
Subject: [TN] BARE PCB disposing

Dear All,

Irrespective of states & countries, what is the best way to dispose the
unpopulated PCBs. We have a large number of Rejected PCBs ready to
dispose. 

regards,

R.Saravanan


PG&E is committed to protecting our customers' privacy. 
To learn more, please visit
http://www.pge.com/about/company/privacy/customer/

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________



****************************************

Like other forms of communications, email communications may be vulnerable to interception by unauthorized third parties.  If you do not wish us to communicate with you by email, please notify us at your earliest convenience.  In the absence of such notification, your consent is assumed.  Should you choose to allow us to communicate by email, we will not take any additional security measures (such as encryption) unless specifically requested. By submitting any personal information to EMX Enterprises Limited or its affiliates, its service providers or agents, you agree, and confirm your authority from any other person whose personal information you submit,  to our collection, use and disclosure of such personal information in accordance with applicable law.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2