Hi JF, You would be best served to get a copy of IPC-6012 and study the specifications for copper thickness in there.Although I have a lengthy PWB history, I think the specifications within are very clear even for those that may not. Best regards, Gerry
> Date: Thu, 28 Feb 2013 11:44:58 -0500
> From: [log in to unmask]
> Subject: [TN] Notes in PCB Fabrication
> To: [log in to unmask]
>
> Hello All!
>
> I'm having a curious note in a fabrication drawing and I would like to
> know if it makes sense.
>
> "1.0oz FINISH (0.5oz COPPER + 0.5oz PLATING)"
>
> And somewhere else in the notes, ENIG is specified...
>
> Ideas?
>
> JF
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________