TECHNET Archives

February 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gumpert, Ben" <[log in to unmask]>
Date:
Fri, 8 Feb 2013 15:11:40 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Larry Dzaugis <[log in to unmask]>
Message-ID:
Subject:
From:
Larry Dzaugis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (71 lines)
Technique matters.
I had 5 lines with TU stations after wave or select soldering.
There was solder splash found 2 ft above the PCA on several stations.

Most of it came from careless cleaning of the solder tip.
One day a solder short came back from the field and large effort made to
get this back under control.
The SMT rework stations had little of the splashes.
The difference was in line vs off line work, less pressure to make rate.
Root cause, too many touch up points.





On Fri, Feb 8, 2013 at 2:42 PM, Gumpert, Ben <[log in to unmask]> wrote:

> Ioan,
>
> My guess is that most 'solder splashing' is a result of the flux activity
> (physical, not chemical). With that in mind, you might look at how much
> flux is being applied and when heat and solder are being applied (all at
> the same time?)
>
> Ben
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
> Sent: Friday, February 08, 2013 2:29 PM
> To: [log in to unmask]
> Subject: EXTERNAL: [TN] Anti-splashing solder wire
>
> Dear Technos,
>
> What do you think about this? Sounds pompous, but I wonder if this
> existed...
>
> We noticed many solder balls and splashes on a particular board, after
> manual soldering or repairs/touch-ups and I wonder if there would be a
> particular brand/model of solder wire which is less splash prone.
>
> Thanks,
>
> Ioan Tempea, ing.
> Ingénieur principal de fabrication / Senior Manufacturing Engineer
> [signature002]<http://www.digico.cc/>
>
> 950 RUE BERGAR, LAVAL, QC, H7L 5A1<http://g.co/maps/2gh3f>
> T+ 1 (450) 967-7100, EXT244
> ------------------------------------------------------------------------
>   [signature001] <http://www.facebook.com/pages/Digico/277076778479>
> ------------------------------------------------------------------------
> Lauréat Dunamis 2012<http://digico.cc/dunamis-2012/>
> Entreprise manufacturière / Gestion du capital humain
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2