That says pretty much the same thing as your first statement.
The most likely way of manufacturing your board will be to drill a bunch of holes in it, prepare the holes for electroplating, plate copper in the holes which will also plate the faces of the panel, then etch the circuit patterns. The plating on the outer layers is normally considered a side effect of the production process. It causes etch resolution issues on very dense designs. But sometimes, because it also reduces trace resistance (both electrical and thermal) is actually required.
It is common to specify at least 0.9 mils (23 microns) on the hole walls, which is a bit greater than your half ounce. If there's enough slop in the specification, the fabricator will favor the hole wall criterion so the board is IPC compliant. (Usually the same thickness deposits on the hole wall as gets plated on the outer layers).
The above explanation only holds for one particular way of building boards, but is the most common way to build cheap, plated boards. Fabricators can be ingenious in figuring out alternate techniques to get whatever the customer specifies.
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Head
Sent: Thursday, February 28, 2013 11:59 AM
To: [log in to unmask]
Subject: Re: [TN] Notes in PCB Fabrication
They want 35 micron finished after plating. Starting copper thickness of the pre-processed material is 17.5 micron and they want it plated up to 35 micron thickness total for the completed fabricated PCB.
James
********************************************************
The information transmitted is intended only for the person or entity to which it is addressed and may contain confidential and/or privileged material. If you are not the addressee, any disclosure, reproduction, copying, distribution, or other dissemination or use of this communication is strictly prohibited. If you have received this transmission in error please notify the sender immediately and then delete this e-mail.
E-mail transmission cannot be guaranteed to be secure or error free as information could be intercepted, corrupted lost, destroyed, arrive late or incomplete, or contain viruses.
The sender therefore does not accept liability for any errors or omissions in the contents of this message which arise as a result of e-mail transmission. If verification is required please request a hard copy version.
********************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|