Good Afternoon:
A question regarding IPC-7711/7721, section 4.3.1 (Conductor Cut, Surface Conductors), details (in Outline section) that cut areas "are sealed with epoxy" and later detail (in Procedure) to "coat the area with epoxy if needed". Seems like a partial contradiction. Any thoughts? Class dependant? End use dependant? Thanks in advance.
Regards,
Steve Vargas