We've just run across a customer's redesign of a PWB adding 0402 resistors. The product has been built for years with a glue and wave process for 0603's to 1210's to IPC-A-610, class 3.
I don't think we can reliably dispense adhesive between pads this close.
Printing adhesive may be an option, but the stencil thickness may limit volume applied for the larger parts.
Finally, we may get solder bridging with 0402's in the wave.
Does anyone have experience with a glue and wave process on 0402's?
Dick Krug, CSSBB, CSMTPE
Senior Process Engineer
Sparton Complex Systems
30167 Power Line Road
Brooksville, FL 34602-8299
p (352) 540-4012 (Internal Ext. 2012)
[log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|