TECHNET Archives

January 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 30 Jan 2013 15:52:29 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
The view to the Stage is clear
The Play and Players are dear
Did the prose and cons we hear
Leave adherence to the plot in fear
Dewey 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, January 30, 2013 8:22 AM
To: [log in to unmask]
Subject: Re: [TN] Gray Thermal Heat Sink Compound-paste

Folks,

   Again I state my inquiry, " Can/theatrically excessive saturation of the SMT components-BGA, etc. devices with the above stated product can a leakage condition".   I don't feel I got an answer.   I am very aware that the placement of the paste should only be over the die surface and with a control volume.    I don't have the brand and/or composition make of the gray material before me, only the aftermath effects of the component /BGA over saturation.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil
Sent: Wednesday, January 30, 2013 9:05 AM
To: [log in to unmask]
Subject: Re: [TN] Gray Thermal Heat Sink Compound-paste

Hi guys,

In our testing the type of thermal paste does not make a difference if the surfaces are really smooth (16 µin or better surface).  Where it makes a difference is in rougher surfaces.  And Brian is right, more is not better.

For electrical isolation we have switch from a thixotropic phase change material (Isostrate) to T-gard with great results.

Just my 2 ¢

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Wednesday, January 30, 2013 9:52 AM
To: [log in to unmask]
Subject: Re: [TN] Gray Thermal Heat Sink Compound-paste

It depends.... on its composition. If it's grey, it may rely on fine metallic powder. I have some Thermaltake TG2 which the makers claim has low electrical conductivity but I suspect it may have metal in it. I use it for CPUs to radiators, so its electrical characteristics are unimportant. Consult the manufacturer's data. BTW, don't put on an excess; if it squeezes out, you're wasting a costly product :(

Brian

On 30/01/2013 15:41, Victor Hernandez wrote:
> Folks,
>
>     Can excessive saturation of the SMT components-BGA, etc. devices with the above stated product can a leakage condition.   Cosmetic wise  it doesn't look pretty.   I am concern functionally over a long period of time.
>
> Victor,
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2