Would ENIG work fine for pogopin applications, versus hard gold? I can see hard gold being required for resistance to wear; but since the pogos just come down and push there should be little sliding movement. Or would hard gold still be a good safe bet, especially if you can see any sort of indentation on the pogo pad from the pogo?
Thanks.