Subject: | |
From: | |
Reply To: | |
Date: | Thu, 6 Dec 2012 08:24:24 +0100 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Wick-tor,
Etching is done in order to eliminate smear, so AFTER etching should be the
answer.Nothing wrong with your logic, In my opinion the order is wrong.
Swap Class 1 and Class 3. Une petitess though.
Inge
On 5 December 2012 20:26, Victor Hernandez <[log in to unmask]>wrote:
> Fellow TechNetters;
>
> When measuring wicking. Is the measurement conducted on a sample
> cross section before a chemical etchant is preformed or after. I get two
> distinct values. Then if I include what is to belief the end of silver
> colored wicking is another. What is the appropriate method? Can someone
> verify the tolerance values printed on each category on the document. It
> appears to me that they are not in the correct order. I have be known to
> be incorrect in my logic.
>
> Victor,
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.