We use step stencils occasionally, maybe 3-4% of stencils.
We use both step down for fine pitch and occasionally step most of the board to use thicker stencil for intrusive solder of a connector.
Dick Krug, CSSBB, CSMTPE
Senior Process Engineer
Sparton Complex Systems
30167 Power Line Road
Brooksville, FL 34602-8299
p (352) 540-4012 (Internal Ext. 2012)
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
Sent: Friday, December 21, 2012 10:33 AM
To: [log in to unmask]
Subject: [TN] Stepped Stencils
Just a poll to see how many assemblers out there are utilizing stepped stencils where a thinner stencil is required for ultra fine pitch or 0201 /
1005 components?
How much of your product mix requires a stepped stencil?
What are the draw backs and pitfalls?
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480 x115
F: 607.266.0482
<mailto:[log in to unmask]> [log in to unmask]
P Please consider the environment before printing this e-mail.
_____
Confidentiality Notice:
This e-mail contains privileged and confidential information which is the property of MPL Incorporated, intended only for the use of the intended recipient(s). Unauthorized use or disclosure of this information is prohibited. If you are not an intended recipient, please immediately notify MPL Incorporated and destroy any copies of this email. Receipt of this e-mail shall not be deemed a waiver by MPL Incorporated of any privilege or the confidential nature of the information.
Export Control:
This message is intended only for the addressee and may contain information that is company confidential or privileged. Any technical data in this message may be exported only in accordance with the U.S. International Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export Administration Regulations (15 CFR Parts 730-774). Unauthorized use is strictly prohibited and may be unlawful. If you are not the intended recipient, or the person responsible for delivering to the intended recipient, you should not read, copy, disclose or otherwise use this message. If you have received this email in error, please delete it, and advise the sender immediately.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|