Hi Victor,
You'd need a nanohardness tester, not microhardness.
------Original Message------
From: Victor Hernandez
Sender: TechNet
To: [log in to unmask]
ReplyTo: TechNet E-Mail Forum
ReplyTo: [log in to unmask]
Subject: [TN] micro hardness tester
Sent: Nov 2, 2012 15:56
Fellow TechNetters;
Any recommendation for checking the hardness of gold plated, >20 micro inches, spring contacts on DIMM connectors, options card connectors and associated cards, PCB?,
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
Regards,
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|