Good Morning Doug,
Thank you for the "spot on" explanation. I should have realized that
you were the chairman on this project and therefore the "go-to" guy.
Unfortunately we have a customer requirement which does not make
reference to IPC-9202 at all but it does require IC to be passed at the
0.9 requirement. I was trying to get an idea of what order of magnitude
others are getting for this parameter but I think I know where we went
wrong (test vehicle coming in contaminated). Garbage in garbage out.
I have to be honest and admit that I need to go read 9203 and get more
familiar with the documentation you have already published. I haven't
been working on cleaning for a long time so I can see I have a lot of
reading to catch up on.
Thanks, as always, for your help.
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, October 09, 2012 5:30 AM
To: TechNet E-Mail Forum; Bavaro, Phillip @ MWG - TW
Subject: Re: [TN] ION CHROMATOGRAPHY - EXCESS CHLORIDE CONTENT
Good morning Phil,
So your candidate process passes ROSE and passes SIR, but "fails" an IC
test. If you use the IPC-9202 criteria, your candidate process
"passes". That is because 9202 is based on SIR as the metric to pass.
IC is taken to benchmark what you have in terms of ionic residues. 9202
does not give a pass or fail for IC data, so this must be from other
studies.
Your testing of controls has shown you what your overall problem is.
Your incoming boards, bought as a commodity item, are not clean. So,
either your pre-cleaning process was not effective, or the chloride
residues of interest are soaked into the assembly and do not come out
except in IC extraction. If you still have some of the as-received
boards, take one and pass it through reflow with no other application of
flux or cleaning. If you see a big jump in residues, you have a problem
with the solder mask.
You ask what you should get, ionic-wise, from a standard water soluble
process. There is no such thing. All fluxes will have their own
interactions with the substrates or materials of construction, which is
why in 9202, if you are qualifying a manufacturing process, the B52 is
made from your intended material set from your intended fabricators.
That way, if you saw the same thing with your polyimide substrate and
your chosen mask and surface finish, then you have a problem with your
fab source, not your process.
Since your process is just over the 0.9 limit you indicate, you can
expect for it to be lower with polyimide, since that has a lower
chloride content.
Doug Pauls
From: Phil Bavaro <[log in to unmask]>
To: <[log in to unmask]>
Date: 10/08/2012 06:31 PM
Subject: [TN] ION CHROMATOGRAPHY - EXCESS CHLORIDE CONTENT
Sent by: TechNet <[log in to unmask]>
________________________________
We have some results that have left me puzzled. We are processing the
IPC B-52 test PWAs using water soluble paste/flux and we can pass the
ROSE test (of course) and the SIR test, but fail the IC test for
excessive choride anion content.
Here is what baffles me.....our control sample is similar and worse than
the test samples.
There seems to be some documentation that the chloride ion might be
related to mishandling and/or soldermask not being properly cured but I
don't have any experience with this test result so I am not sure how to
respond to that (hopefully Terry will chime in on this). We processed
all the samples using the proper gloves and bags and doubt that we
contaminated them.
We are trying to meet the requirement of 0.9 micro-gm/cm-cm maximum and
our failing control sample is 3.36, one test sample is 4.67, and the
other two samples are running at .91 and .90. What value for chloride
anion content does a normal WS process yield? Are these numbers way out
of range for normal test results or is chloride always a pesky result?
I am looking for the answer to the question "is this really a problem?"
The control sample was washed but did not have any paste applied to it
at all. The test samples were run through the full assembly reflow
process then cleaned and Rose tested before shipment to the lab.
All the rest of the results for the IC test are passing so I don't know
quite how to proceed from here.
My current plan is to run another set of tests with more than one
control sample, and then to simulate various phases of clean (IOW barely
cleaned, half cleaned, and then a couple of fully cleaned samples). As
I am not really familiar with IC test results, I want to see the what
the constituents of the "dirt" really look like from an IC test
perspective as well as repeat the previous test results.
One item I have noted is that we did not have our chosen board supplier
build these boards but instead bought these off the shelf from one of
the dummy component suppliers. But the thought was that as long as they
were cleaned using our normal process, they should be acceptable.
These particular test samples use FR4 and not the high Tg polyimide that
most of our PWBs are built from.
Any comments on this would be appreciated.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|