TECHNET Archives

October 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 10 Oct 2012 17:45:44 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Message-ID:
Subject:
From:
Ioan Tempea <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (58 lines)
Wow,

That's why I'm addicted to TN: quick and priceless answers.

We are users of the Trace pens, but they work too slowly for this application.

Foam Q-tips, good lead, will try again to push them, as last time around, the price made them not eligible.

Contacted Crystal Mark for info, waiting for them to answer, but can't trace CCRD on the Internet. Actually I'm asking myself questions, knowing the suggestion comes from Doug and the first search result is about nanoparticles delivering drugs into brain... ;-)

Thanks again,

Ioan Tempea
Ingénieur principal de fabrication / Senior Manufacturing Engineer


950 RUE BERGAR, LAVAL, QC, H7L 5A1
T+ 1 (450) 967-7100, EXT244
------------------------------------------------------------------------
  
------------------------------------------------------------------------
Lauréat Dunamis 2012
Entreprise manufacturière / Gestion du capital humain


Dear Technos,

We need to locally strip the acrylic coating (1B31S) from a few components, on a few thousands of boards. Right now we're using Q-tips to do the rubbing and, besides having to pluck tons of fibers afterwards, we're also going through a lot of Q-tips.

So the question is: is there anything else we can use, that will be more effective, cleaner and more economical?

Thank you,

Ioan Tempea
Ingénieur principal de fabrication / Senior Manufacturing Engineer [signature002]<http://www.digico.cc/>

950 RUE BERGAR, LAVAL, QC, H7L 5A1<http://g.co/maps/2gh3f>
T+ 1 (450) 967-7100, EXT244
------------------------------------------------------------------------
  [signature001] <http://www.facebook.com/pages/Digico/277076778479>
------------------------------------------------------------------------
Lauréat Dunamis 2012<http://digico.cc/dunamis-2012/>
Entreprise manufacturière / Gestion du capital humain


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2