Well then, let my nano-particle augmented brain assist.
I actually spelled it wrong. It is CCRCo, LLC. Hal Horrocks, the
President of the company, gave a very good presentation on media removal
at one of the previous SMTA/IPC Cleaning and Coating Conferences. He
indicated then that most military depots are going to media blasting vs.
chemical removal, in order to decrease chemical usage and hazardous waste.
You can contact Hal at [log in to unmask] or 800-443-2726. They also have a
web site at www.ccrco.com.
I plan on getting one of his machines to play with should the Capital
Fairy ever sprinkle Magic Capital Equipment Dust on my request.
Doug Pauls
From: Ioan Tempea <[log in to unmask]>
To: <[log in to unmask]>
Date: 10/10/2012 12:47 PM
Subject: Re: [TN] Conformal coating removal
Sent by: TechNet <[log in to unmask]>
Wow,
That's why I'm addicted to TN: quick and priceless answers.
We are users of the Trace pens, but they work too slowly for this
application.
Foam Q-tips, good lead, will try again to push them, as last time around,
the price made them not eligible.
Contacted Crystal Mark for info, waiting for them to answer, but can't
trace CCRD on the Internet. Actually I'm asking myself questions, knowing
the suggestion comes from Doug and the first search result is about
nanoparticles delivering drugs into brain... ;-)
Thanks again,
Ioan Tempea
Ingénieur principal de fabrication / Senior Manufacturing Engineer
950 RUE BERGAR, LAVAL, QC, H7L 5A1
T+ 1 (450) 967-7100, EXT244
------------------------------------------------------------------------
------------------------------------------------------------------------
Lauréat Dunamis 2012
Entreprise manufacturière / Gestion du capital humain
Dear Technos,
We need to locally strip the acrylic coating (1B31S) from a few
components, on a few thousands of boards. Right now we're using Q-tips to
do the rubbing and, besides having to pluck tons of fibers afterwards,
we're also going through a lot of Q-tips.
So the question is: is there anything else we can use, that will be more
effective, cleaner and more economical?
Thank you,
Ioan Tempea
Ingénieur principal de fabrication / Senior Manufacturing Engineer
[signature002]<http://www.digico.cc/>
950 RUE BERGAR, LAVAL, QC, H7L 5A1<http://g.co/maps/2gh3f>
T+ 1 (450) 967-7100, EXT244
------------------------------------------------------------------------
[signature001] <http://www.facebook.com/pages/Digico/277076778479>
------------------------------------------------------------------------
Lauréat Dunamis 2012<http://digico.cc/dunamis-2012/>
Entreprise manufacturière / Gestion du capital humain
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|