Hi, Joyce
What is rp system?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Monday, October 15, 2012 11:16 AM
To: [log in to unmask]
Subject: Re: [TN] board baking - thread continuation
GDAIS Security Warning: This message was delivered from the Internet. Be cautious about trusting the content, particularly any links or attachments. If there is any doubt as to the authenticity, forward this email as an attachment to [log in to unmask] for analysis prior to opening any attachment or link.
________________________________
Add "rp system" pack into your sealed moisture barrier bag to ensure limited oxidation.
--------------------------
Sent using BlackBerry
----- Original Message -----
From: Glen Herzog [mailto:[log in to unmask]]
Sent: Monday, October 15, 2012 12:09 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] board baking - thread continuation
Good to hear from you,
A thorough simple taping would probably work. However, it is much more difficult to be confident that employees are taping properly. Heat sealing, as I indicated is easy and the sealing equipment is only @$200-$300. Sometimes employees are more responsible when they know management is serious. Actually, you could use a "Seal-a-Meal" sealing machine. However, I would be embarrased to tell that to customers or management.
Glen
________________________________
From: Robert Kondner <[log in to unmask]>
To: TechNet E-Mail Forum <[log in to unmask]>; Glen Herzog <[log in to unmask]>
Sent: Mon, October 15, 2012 10:35:09 AM
Subject: RE: [TN] board baking - thread continuation
Hi,
According to content on some sites simple taping might be OK and heat seal not required.
I wonder how moisture diffusion through an incomplete tape seal and a bend compares to bag surface diffusion.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glen Herzog
Sent: Monday, October 15, 2012 12:10 AM
To: [log in to unmask]
Subject: Re: [TN] board baking - thread continuation
Joyce Koo recommended a dry box. I agree that that is recommended, especially for short term use such as you've used some of the components and you will use the rest in a few days to a few weeks. However, if you need longer term storage I recommend purchasing moisture barrier bags, desiccant and moisture indicator cards. They're relatively inexpensive. You would need a heat sealer ($200-$300 and simple to use) I would not worry about vacuuming the bag, it's probably not worth the effort. The formula for how much desiccant to use depends on what desiccant is used. For example you might take look at:
http://texastechnologies.com/moisture-control/desiccant/silica-gel/packaged/sorb-it-silica-gel-unit-size.htm
for one example. I have no investment in that company, it's just a reference to an example.
Good luck
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|