TECHNET Archives

October 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 10 Oct 2012 18:29:25 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (76 lines)
A light swabbing of toluene will ensure you don't have any residues, anywhere. Not even inside of your casket.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, October 10, 2012 1:03 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal coating removal

GDAIS Security Warning:
This message was delivered from the Internet. Be cautious about trusting the content, particularly any links or attachments.

If there is any doubt as to the authenticity, forward this email as an attachment to [log in to unmask] for analysis prior to opening any attachment or link.

Dewey,
Will I don't disagree, stripping of an entire assembly, especially if you have thousands, is incredibly wasteful and often causes as many problems as it solves.  Global stripping involves immersion in toluene or xylene and creates a LOT of flammable waste and often gets into other connectors and keep out zones where it causes problems.  The media blasting is a dry process and the residues easily removed.  I would suggest a light toluene swab of the area anyway to make sure that you don't have any residual coating on the pads that would interfere with a good solder joint.

Doug Pauls



From:   "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   10/10/2012 12:17 PM
Subject:        Re: [TN] Conformal coating removal
Sent by:        TechNet <[log in to unmask]>



I would wait for Doug on this, since he takes his lead from Graham on sartorial splendor and is more used to partially coated affairs. I would strip the whole assembly if possible as the process does an excellent job of prepping the substrate for re-coating.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Wednesday, October 10, 2012 9:56 AM
To: [log in to unmask]
Subject: [TN] Conformal coating removal

Dear Technos,

We need to locally strip the acrylic coating (1B31S) from a few components, on a few thousands of boards. Right now we're using Q-tips to do the rubbing and, besides having to pluck tons of fibers afterwards, we're also going through a lot of Q-tips.

So the question is: is there anything else we can use, that will be more effective, cleaner and more economical?

Thank you,

Ioan Tempea
Ingénieur principal de fabrication / Senior Manufacturing Engineer [signature002]<http://www.digico.cc/>

950 RUE BERGAR, LAVAL, QC, H7L 5A1<http://g.co/maps/2gh3f>
T+ 1 (450) 967-7100, EXT244
------------------------------------------------------------------------
  [signature001] <http://www.facebook.com/pages/Digico/277076778479>
------------------------------------------------------------------------
Lauréat Dunamis 2012<http://digico.cc/dunamis-2012/>
Entreprise manufacturière / Gestion du capital humain


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2