TECHNET Archives

October 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 23 Oct 2012 08:58:26 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "McGrath, Jim" <[log in to unmask]>
Message-ID:
Subject:
From:
"McGrath, Jim" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (95 lines)
Victor, here's the attachment. 


Jim McGrath
Strategic Marketing Manager
TE Consumer Devices
Cell: 630-244-3872
Email: [log in to unmask]

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Tuesday, October 23, 2012 6:23 AM
To: [log in to unmask]; McGrath, Jim
Cc: [log in to unmask]
Subject: RE: Ni barrier thickness

Jim,

   Your attachment was strip off by TechNet.   Can you send off line to me.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McGrath, Jim
Sent: Monday, October 22, 2012 4:04 PM
To: [log in to unmask]
Subject: Re: [TN] Ni barrier thickness

See attached JEDEC Mechanical Outline for DDR3 DIMM memory module. Page 17 shows recommended plating and Ni barrier.

 


Jim McGrath
Strategic Marketing Manager
TE Consumer Devices
Cell: 630-244-3872
Email: [log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, October 22, 2012 2:40 PM
To: [log in to unmask]
Subject: Re: [TN] Ni barrier thickness

No, that information belongs on the SCD for the component.
There are so many different applications with different requirements so there is no standard that could cover them all.
Even PWBs plated with gold must have the exact dimensions/methods documented on the fabrication drawing if they are outside of the ENIG standard.
However, there are some plating specifications in the JEDEC component standards.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, October 22, 2012 2:33 PM
To: [log in to unmask]
Subject: [TN] Ni barrier thickness

GDAIS Security Warning: This message was delivered from the Internet. Be cautious about trusting the content, particularly any links or attachments. If there is any doubt as to the authenticity, forward this email as an attachment to [log in to unmask] for analysis prior to opening any attachment or link.
________________________________


Dear Technos,

For applications other than ENIG, like, for instance, gold plated Cu pins, is there any standard (ASTM?) specifying the thickness of the Ni barrier that would prevent Cu diffusion towards the surface?

Thank you,

Ioan Tempea, ing.
Ingénieur principal de fabrication / Senior Manufacturing Engineer [signature002]<http://www.digico.cc/>

950 RUE BERGAR, LAVAL, QC, H7L 5A1<http://g.co/maps/2gh3f>
T+ 1 (450) 967-7100, EXT244
------------------------------------------------------------------------
  [signature001] <http://www.facebook.com/pages/Digico/277076778479>
------------------------------------------------------------------------
Lauréat Dunamis 2012<http://digico.cc/dunamis-2012/>
Entreprise manufacturière / Gestion du capital humain


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2