Hi Ben,
How are you applying the material and what components are you seeing this on?
There are some application tricks to the trade to minimize this phenomenon.... You can contact me offline if you'd like to discuss this further.
Otherwise, I'd recommend you speak to both Matt Eveline at HumiSeal and Jon Urquhart at PVA, both great resources to get you going in the right direction.
Best Regards,
Phil
+44 7703 795422
Sent from my iPhone
On 3 Oct 2012, at 22:47, Lee Hitchens <[log in to unmask]> wrote:
> Hi Ben what are you comparing too? A solvent based coating or something else! Is the coating running during or just after application or during the cure process under the uv lights where it can get hot?
>
> Best regards
>
> Lee hitchens
>
> Sent from my iPad
>
> On 3 Oct 2012, at 21:39, "Gumpert, Ben" <[log in to unmask]> wrote:
>
>> Technetters,
>>
>> I'm evaluating Humiseal's UV40 conformal coating, but I'm seeing wetting issues - where the coating completely runs off of vertical lead surfaces.
>>
>> I see from some e-mails a couple of years ago that some of you are using this coating material, or were looking into it. Is anyone else seeing this problem, or have some suggestions to fix?
>>
>> Ben
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|