TECHNET Archives

October 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 17 Oct 2012 13:08:56 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="US-ASCII"
From:
Douglas Pauls <[log in to unmask]>
Parts/Attachments:
text/plain (21 lines)
Good afternoon all,

I wonder if any of you know of  a heat shrinkable sleeving that would be 
in the static dissipative range for volume resistivity?  This would be 
between 1E6 and 1E9 ohm-cm.  Most of the ones that I am aware of are 1E11 
ohm-cm or higher.

I don't know of any, so I thought I would turn to my favorite forum. 

The application is paint brush handles.  Since most brushes are painted 
wood, they can generate static.  We thought having a shrinkable ESD cover, 
vs. some of the liquid coatings, would be a possible solution.

Doug Pauls


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2