TECHNET Archives

September 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Larry Dzaugis <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Larry Dzaugis <[log in to unmask]>
Date:
Thu, 13 Sep 2012 10:07:39 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (16 lines)
Is this purchased solder or is solder from their own machines and reclaimed
from the dross?

A factory that uses one solder alloy is at a low risk of  cross
contamination.
I would add checking the recast solder from the reclamation machine if used
on site to verify the alloy.

Larry Dzaugs


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2