Richard,
Could you elaborate on your statement about avoiding lead-rich regions with the SJ? Without knowing better one could get the impression that lead-rich regions are going to cause reliability problems but we all know that SnPb solder joints do have lead-rich regions and they are certainly reliable. Isn't the problem due more to alignment of lead-rich regions at an interface when you don't have good mixing between Pb-Free and SnPb solder?
Regards,
George
George M. Wenger
Senior Principal Reliability / FMA Engineer
Andrew Corporation - Wireless Network Solutions
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 Office (732) 309-8964 Mobile
E-mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, September 26, 2012 11:11 AM
To: [log in to unmask]
Subject: Re: [TN] Using Tin/Lead balled BGA in a Lead-Free process
Vladimir is correct, the key is to avoid lead-rich regions within the SJ.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Wednesday, September 26, 2012 10:07 AM
To: [log in to unmask]
Subject: Re: [TN] Using Tin/Lead balled BGA in a Lead-Free process
Peter,
The rules are still the same: Pb has to be evenly distributed throughout the balls.
Regards,
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: Peter Barton <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Wed, 26 Sep 2012 15:45:00
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
Peter Barton
<[log in to unmask]>
Subject: [TN] Using Tin/Lead balled BGA in a Lead-Free process
Hi Technetters,
Interesting that this question has arisen for me when there has been a question posed here on the reverse scenario in the last couple of days. Firstly, I agree with other posters that full reflow and alloy mixing must be achieved when using Lead free BGA's in a Tin Lead process. There is quite a lot of data out there supporting this.
My problem is finding research data on using a Tin/Lead BGA on an otherwise fully Lead free assembly. This appears to be much more limited. So far I have only found one paper that refers to this particular scenario and some of it's conclusions are carefully qualified.
Assuming that all the other the packaging materials for the Tin/Lead BGA part in question are capable of surviving a suitable reflow process to successfully solder the lead free parts whilst minimising thermal input, can anyone out there comment on potential reliability issues. For information the BGA balls are 63/37 Sn/Pb and the solder paste alloy is SAC305.
Many thanks in advance,
Peter Barton
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|