Will something like plain ol' acetic acid [vinegar], or a mild lye [NaOH]
also work?
I remember lecturing operators on how even spittle will take the [Al] bond
pads off an IC. I know it is not the same aluminum, but HF is certainly
nasty stuff and would heed Joyce's cautions
Steve Creswick
Sr Associate - Balanced Enterprise Solutions
http://www.linkedin.com/in/stevencreswick
616 834 1883
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Thursday, September 06, 2012 4:55 PM
To: [log in to unmask]
Subject: Re: [TN] Aluminum Etch
Electrochemical polishing plus HF etching. Not nice. My 2 cents (wear
double gloves. I got nasty burn before... thanks god I got live to tell the
story --- when I was young and stupid).
Joyce Koo
Materials Researcher - Materials Interconnect Lab Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Thursday, September 06, 2012 4:21 PM
To: [log in to unmask]
Subject: [TN] Aluminum Etch
Fellow TechNetters:
Any suggestion on an etchant for aluminum, Al 5052 H32 , for grain
structure delineation after cross section and final polish?
Victor
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|