I agree that a very strong halide flux is essential for pretinning, but
you may need more for any alloy more resistant than 18/8/3, including
ultrasound to break up that ornery refractive oxide.
Brian
On 28/09/2012 18:28, Paul Edwards wrote:
> Torsten,
>
> The last time I did this type of thing I did the following:
>
> Pre-tin S/S soldering areas with the same solder metallurgy as your solder paste using a very active acid flux (I used a hydrobromic acid type flux), wash thoroughly, then place on PCB like regular component and/or RF shield...
>
> Some adjustment need to be made depending (that word again...) on the joint configuration and part...
>
> Paul
>
> Paul Edwards
> Process/Quality Engineering
> Surface Art Engineering
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Torsten Hagge
> Sent: Friday, September 28, 2012 8:17 AM
> To: [log in to unmask]
> Subject: [TN] soldering stainless steel
>
> Hi all,
>
> has anybody experience with soldering stainless steel parts directly on a PCB? What solder process work fine?
>
> Application is a medical sensor with body contacts.
>
> Torsten
>
>
> Kind regards
>
> KRISTRONICS GmbH
> Torsten Hagge
> Gewerbegrund 5-9
> 24955 Harrislee
> Telefon +49 (0) 461 7741-624
> Telefax +49 (0) 461 7741-642
> [log in to unmask]
> www.kristronics.de
>
> Meet at electronica 2012, A6, 409
>
> Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL
> Gesch�ftsf�hrer Dipl.-Ing. oec. Thormod Ohm
> Ust-Id-Nr. DE 811182059
> Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ 21570011
> IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|