Oh we have understood your question slightly differently.
Thanks for clarifying.
There isn't a text book answer to your question, I leave others/users to
state their preference and why. The answer lies in your evaluation of the
balance of risks and benefits, either of which can be hard to quantify.
Water soluble fluxes probably present a simpler cleaning process than no
clean, but the consequences for not cleaning properly are probably worse,
and for missed cleaning are certainly worse. Delayed cleaning can be an
issue with water wash products.
Water soluble fluxes can be much more active than no cleans (but not
invariably) and this could be an advantage when soldering.
A lot of the answers will be supplier specific, especially if you move from
no clean which all meet common specifications irrespective of supplier.
Water wash products are more proprietary.
It would help people to answer if you could give a little more background:
Do you just hand solder or do you have reflow/wave /other? What are you
running there?
After soldering, what processes do you have? Cleaning, coating, probing etc?
Does your product have to meet any industry (customer)specific requirements?
For example often medical equipment is conformally coated.
Regards
Mike Fenner
Bonding Services & Products
M: +44 [0] 7810 526 317
T: +44 [0] 1865 522 663
E: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Mahoney
Sent: Monday, September 24, 2012 1:14 PM
To: [log in to unmask]
Subject: Re: [TN] IPC Standard Temperature Profile for RoHS Pb Free Solder
(Hand Soldering)?
Questions:
We are producing a volume High end medical 4 lyr rigid flex assembly. My
question is which soldering process would be considered best?
1) No clean soldering process
2) Water soluble process
Thank you, Jim Mahoney
Mass Design Inc.
Applications Engineer
P# 603-886-6460 X215
DDTC Registered and ITAR Compliant
ISO 9001:2008 Certified
? Please consider the environment before printing this e-mail
Confidentiality Notice: This page and any accompanying documents contain
information that is confidential, privileged or exempt from disclosure and
is intended for the exclusive use of the addressee. If you are not the
intended recipient, you are hereby notified that any disclosure, copying,
distribution or use of the contents of this information in any manner is
strictly prohibited.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|