Seems awful high (20 ug/in2?) for an acetate from the bag. You may be
seeing a front end eluter coming out at the same time as formate, leading
to the high numbers. You would either have to use a different method to
check, or use a different analytical approach, such as FTIR to check.
Doug Pauls
From: Richard Kraszewski <[log in to unmask]>
To: <[log in to unmask]>
Date: 09/11/2012 11:33 AM
Subject: Re: [TN] Source of IC Contamination Species
Sent by: TechNet <[log in to unmask]>
I am speaking pretty generally. Sometimes I see them get reported other
times not (ND).
For an example WOA levels may be~ 10 ugm/in2 whereas formate acetates
maybe twice that level.
Extraction would be your typical IPA/H2O in a sealed bag floated on a
water bath for 1 hour.
Rich Kraszewski
(920)969-6075
-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]]
Sent: Tuesday, September 11, 2012 11:21 AM
To: 'TechNet E-Mail Forum'; Richard Kraszewski
Subject: RE: Source of IC Contamination Species
Where you found those? Extracted at high temperature overnight? What else
on the board?
Joyce Koo
Materials Researcher - Materials Interconnect Lab
Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Tuesday, September 11, 2012 12:10 PM
To: [log in to unmask]
Subject: [TN] Source of IC Contamination Species
Occasionally, IC analyses are reported to have elevated levels of acetates
and formates. Is it the general consensus that source of these
contamination is assumed to be the decomposition of larger molecular
weight weak organic acids found in soldering fluxes? I can't imagine that
any manufacturer would actually be placing acetic or formic acids directly
into a flux formulation. These are much too volatile and aggressive.
Thoughts?
Rich Kraszewski
Senior Process Engineer
PLEXUS
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|