We kept getting dead batteries, until someone realized what they were doing. We re-educated them that some components (batteries) need to remain in their original packaging. They were just trying to follow their procedure.
This all started some years back because we bought from a specific vendor custom metal can ultra-high gain CMOS opamps that had NO front end static protection, they came packaged with a hair fine spring wound around their leads from the vendor. The "receiving person" thinking the spring was a piece of scrap removed it, each amp was in the neighborhood of 4K apiece, and they trashed a number of them, I think somewhere upwards 50, it has been 20 years. These are used as the front end of a radiation monitoring instrument and are custom built and selected for their characteristics, production runs of the amps are about every 10 years they will make a few thousand and put them on a shelf.
So soldering these things in is a joy too, you place them in their holders dead bug style, solder each of the leads on, then unwind the springs without breaking anything, then test the amp in a high rad source test pig to verify their calibration, about 8 hrs per instrument, if they pass....
We (I&C) raised all kinds of points about electronic component handling ... So they wrote a procedure!
pat
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Tuesday, August 14, 2012 9:54 AM
To: [log in to unmask]
Subject: Re: [TN] PCBA shelf life
Pat,
I 'like' the idea of storing batteries in conductive foam... How did that work out? Was the shelf life found to be not quite what was expected??
Sometimes people do the silliest things, sadly, with good intentions....
They live among us...
Steve Creswick
Sr Associate - Balanced Enterprise Solutions http://www.linkedin.com/in/stevencreswick
616 834 1883
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Tuesday, August 14, 2012 12:31 PM
To: [log in to unmask]
Subject: Re: [TN] PCBA shelf life
I have a little experience in this area.
We have an onsite warehouse that has our ready spares stored within. We
are located on a bluff 85' above the Pacific Ocean. We have boards stored
in the warehouse over 20 years old and some in their 30's and even 40's.
Moisture is an issue, as is the salt air corrosion, one of the storage areas is an "E" room controlled at 68 deg. F and at a 40%RH (sort of) the air is
unfiltered. The room has 2 large rollup doors to facilitate material
handling. This is for the boards or modules that are graded
"Quality" or "Important to Safety", for all other spares they are stored in
an open bay 100000 sq.ft. warehouse. When we 100% inspect boards prior
to use we find, degraded solder, corrosion on traces, rusty component leads.... the list goes on, when repairs are attempted we usually end up
with measling around the soldered area. One of the ways we have minimized
damage is baking the boards in a desiccant oven or heating them with a hot
air gun at low temperature to bake out the moisture entrained. Most of
these OLD boards are of 68-80 vintage, single sided, fiberglass boards.
Storage may be is in bins or shelves in open ended anti-stat bags, (if they have been looked at in recent times), just in bubble wrap, plastic bags, paper wrap, sometimes in ziploc style anti-stat bags, and sometimes on open shelves in cardboard boxes, depending on when it was last accessed and who
did it. We are not allowed to store them in bags with desiccant bags
because the storage facility doesn't have neither the manpower to deal with maintaining the desiccant nor the "environmental hazards" associated with
it, (My box of soap to stand on).
We inspect every piece of equipment to 100% prior to installation and under magnification just to be sure, most items are burned-in for 72 hours prior
to installation.
When they get NEW boards/components, they are OPENED by QA to receipt inspect them and remove any foreign material, useful manuals, special tooling, desiccant.... and are put on the shelf without resealing (in most
cases) the original packing, if it is retained at all, and no manuals,
special tooling, etc., (sorry my box again).
I think I may site some mentioned IPC standards to our overseers, although it only took 20 years for them to start putting ALL electronic components in anti-stat bags or foam before delivery.
They did store lithium backup batteries in conductive foam though, they looked like chips and they wanted to get them off of the wax-coated
cardboard they came in, but that's another story.
Pat Goodyear
Control Technician
Pacific Gas and Electric
Diablo Canyon Nuclear Power Plant
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Tuesday, August 14, 2012 5:56 AM
To: [log in to unmask]
Subject: Re: [TN] PCBA shelf life
HI
In storage the bare boards will suffer from ingress of moisture and loss of
solderability, the longer you keep them the more they are affected. Baking
the boards to dry them can/will degrade solderability.
Properly packed and stored unopened in original packaging per IPC
recommendations, industry wisdom would be something like: expect to see up
to a year for most finishes. Exceptions are immersion tin and some OSP which
will only go 6 months Probably the longest lasting finish would be Sn/Pb
HASL.
NO doubt others will have opinions and probably someone will have stored
PCBS for some outrageously long period OK :) What you actually get is an it
depends - not just on the quality and type of finish, but on the criticality
of your own designs and processes as well as how stored.
IOW, in a perfect world you would work out what you can or can't do. In this
world... this topic is a perennial favorite and you will find many
references in the TechNet archive.
Anyway first look at IPC standards, there is one for just about everything
you can think of. 1601 for board storage and J-003 for board solderability
testing would be good places to start. These will help you Either determine
what you should be doing; or confirm that what you are doing is correct.
Regards
Mike Fenner
Bonding Services & Products
M: +44 [0] 7810 526 317
T: +44 [0] 1865 522 663
E: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ivan Feng
Sent: Tuesday, August 14, 2012 2:22 AM
To: [log in to unmask]
Subject: [TN] PCBA shelf life
Folks,
Bare PCB has a shelf life depending on its surface finish, component like
electrolytic capacitor and MSD devices also have defined shelf life.
But for PCBA, how to define its shelf life? Is there any applicable
standards?
Any suggestions are welcomed.
Regards
Ivan
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
PG&E is committed to protecting our customers' privacy.
To learn more, please visit
http://www.pge.com/about/company/privacy/customer/
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
PG&E is committed to protecting our customers' privacy.
To learn more, please visit http://www.pge.com/about/company/privacy/customer/
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|