TECHNET Archives

August 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Reid <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Reid <[log in to unmask]>
Date:
Wed, 15 Aug 2012 13:55:28 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (81 lines)
I always have to warn those who bake to get rid of delamination that it
rarely works. The delamination will probably still be with you after the
bake. 

How do you know that you have delamination? Is it visible?


Sincerely,  

 

Paul Reid 

Program Coordinator  

PWB Interconnect Solutions Inc. 
235 Stafford Rd., West, Unit 103 
Nepean, Ontario Canada, K2H 9C1 

613 596 4244 ext. 229  

Skype paul_reid_pwb 
[log in to unmask] 

 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: August 15, 2012 10:40 AM
To: [log in to unmask]
Subject: [TN] bare board pre-bake parameters

Good morning all,

We have recently had some boards delaminate and are considering
pre-baking as a possible solution.  I need to know some "rules of thumb"
for pre-bake time and temperature, suggested atmosphere (dry nitrogen?),
allowable time between pre-bake and soldering.

At the moment I only have minimal information on the boards so I don't
know their physical size, number of layers or if they are SMT or PTH.

I realize it could be a bad batch and the problem may only be with one
group of boards as this is not a common problem with boards form many of
our fab houses or CMs.

Thanks in advance,

Phil Nutting
Design for Manufacturing Engineer
Kaiser Systems, Inc.
126 Sohier Road
Beverly, MA 01915
Phone: 978-922-9300 x1310
Fax: 978-922-8374
e-mail: [log in to unmask]<mailto:[log in to unmask]>
www.kaisersystems.com<http://www.kaisersystems.com>
www.linkedin.com/in/philnutting<http://www.linkedin.com/in/philnutting>


________________________________
Note: All the information contained in this e-mail and its attachments
is proprietary to Kaiser Systems, Inc. and it may not be reproduced
without the prior written permission of sender. If you have received
this email in error, please immediately return it to sender and delete
the copy you received.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2