Hi Rudy,
You are with one correction: the percentage of Co or Ni in hard Au is very small (may be lower then a single digit).
Regards,
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: R Sedlak <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Tue, 14 Aug 2012 11:43:17
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
R Sedlak
<[log in to unmask]>
Subject: [TN] Hard vs. Soft gold
It is my understanding that both hard and soft gold are electroplated.
The difference is that "soft gold" is essentially pure, whereas "hard gold" is highly alloyed, often with Cobalt, to harden it.
Rudy Sedlak
RD Chemical Company
--- On Tue, 8/14/12, Guy Ramsey <[log in to unmask]> wrote:
From: Guy Ramsey <[log in to unmask]>
Subject: Re: [TN] PCB finish: ENIG vs. hard gold
To: [log in to unmask]
Date: Tuesday, August 14, 2012, 11:32 AM
I am not sure I can talk to hard or soft gold, and suitability for
soldering.
But, I can say that it is possible to solder to electroplated gold, which is
different from Immersion Gold finish.
I think some people say hard gold when they mean electroplated gold.
There is a brief discussion of this in Coomb's Handbook.
Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Tuesday, August 14, 2012 12:12 PM
To: [log in to unmask]
Subject: [TN] PCB finish: ENIG vs. hard gold
Hi everyone,
We have a PCB supplier who is offering "Hard Gold" as an alternate to ENIG
finish, due to PCB size and processing capabilities. The application is
Class 3 (mil/aero). The circuit is thin FR4 and subject to SMT reflow w/
Sn63Pb37 (non RoHS) solder alloy, and moderate flexing in end application.
Can anyone offer info on the differences between the two finishes, and/or
their suitability? Is there an IPC spec (or specs) that outline "hard
gold"?
Thanks,
Kevin Glidden
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|