Hi Bill,
Check out UPE:
http://www.upe-inc.com/production-capabilities/
They do some of the heaviest copper that I've seen, and they've been doing
it for years...
Steve
-----Original Message-----
From: [log in to unmask]
Sent: Thursday, August 23, 2012 7:37 PM
To: [log in to unmask]
Subject: [TN] Heavy Copper PCB Houses
TechNetters: Could some of you folks provide some PCB Houses that routinely
produce multilayer PCBs with heavy copper (Cu weight
around 16 oz/ft2).
Thanks in advance for your assistance.
THANKS AGAIN,
Bill Black
Medco
631-667-9699 X13
[log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________