TECHNET Archives

August 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Thu, 9 Aug 2012 15:56:24 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (88 lines)
Wow. Sweet.  Many thanks.  

Joyce Koo
Materials Researcher - Materials Interconnect Lab
Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Thursday, August 09, 2012 11:35 AM
To: [log in to unmask]
Subject: Re: [TN] pin in paste

I don't think anyone mentioned it,
(and I'm not sure how "real-world" useful it is)
but Bob Willis offers a FREE introductory tutorial 
on Pin-In-Hole-Reflow published by 007 
here:

http://pihrtechnology.com/

Jack

.
On Wed, 8 Aug 2012 08:24:20 +0100, Mike Fenner <[log in to unmask]> wrote:

>HI Joyce
>There is plenty of useful stuff available, if you search (including on the
>usual suppliers' websites) for 'pin in paste' or 'Pin in hole reflow' or
>'Intrusive reflow' you will catch a number of pragmatic and some theoretical
>studies.
>It is possible to not to have drips, push through etc of paste and solder
>void free with good hole fill.
>What you can do depends on the connector/board design, but generally you are
>looking to offset the paste on printing rather than print into the hole. On
>reflow it will wet in. If you need to augment the solder volume because
>there isn't enough space on board area then you may be able to use component
>shaped preforms in tape and reel presentation. Just P&P in to the paste as
>if a component. This is relatively standard presentation for a number of
>apps not just PIP, so is relatively inexpensive. You can P&P washers in the
>same way with appropriate tooling although at lower volumes this can be
>expensive if you need an exotic size in low volumes, due to taping costs. At
>lower volumes still you can use daisy chains.
>
>
>
>Regards
>
>
>Mike Fenner
>
>Bonding Services & Products
>M: +44 [0] 7810 526 317
>T: +44 [0] 1865 522 663
>E: [log in to unmask]
>
>
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
>Sent: Tuesday, August 07, 2012 10:04 PM
>To: [log in to unmask]
>Subject: [TN] pin in paste
>
>Joyce Koo
>Materials Researcher - Materials Interconnect Lab
>Research In Motion Limited
>Office: (519) 888-7465 79945
>Mobile: (226) 220-4760
>
>Hi, Calling on all of the gurus, Anyone has one or two good reference
>regarding voiding minimization or voiding elimination for pin in paste?
>Hopefully it is not in need of using performs.  Many thanks for all your
>help.
>Best regards,
>            joyce

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2