I did not read the whole article. But I thought the purpose of WEEE (predecessor to RoHS) was to force recycling and reuse of electronic waste. Isn't tin being reclaimed and reused? Or is that reclaimed tin just too expensive, as compared to virgin tin?
Shawn Upton, KB1CKT
Test Engineer
Allegro MicroSystems, Inc
[log in to unmask]
603.626.2429/fax: 603.641.5336
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of harvey
Sent: Saturday, August 25, 2012 9:32 PM
To: [log in to unmask]
Subject: [TN] re TIN---an important article
http://www.businessweek.com/articles/2012-08-23/the-deadly-tin-inside-your-ipad
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________