TECHNET Archives

July 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 5 Jul 2012 09:24:52 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (58 lines)
Hi Neil - before you go down that road, I recommend you determine the root 
cause of the dendritic growth. You may be able to eliminate the issue with 
other methods than tenting the vias which may be more advantageous or 
lower cost.  Tenting the vias could make the situation worst depending on 
what is causing their initiation and growth. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Neil Atkinson <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
07/04/2012 11:02 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
<[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Copper Dendrites






 

 What is the view of covering vias with solder resist to prevent dendrite 
growth?

This is an FR4 PCB with OSP finish, SMT reflow both sides and a few 
through hole components soldered with a selective soldering process...

Thanks in anticipation of the help of the Technet!

Neil


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2