TGASIA Archives

July 2012

TGAsia@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
multipart/mixed; boundary="_002_1E8EEA5549586744B337DF81BB4AC78413317F3D34nts482kiikimb_"
X-To:
Date:
Wed, 1 Aug 2012 12:54:14 +0800
Reply-To:
Eileen Xiang <[log in to unmask]>
Subject:
From:
Eileen Xiang <[log in to unmask]>
Message-ID:
MIME-Version:
1.0
Sender:
Parts/Attachments:
text/plain (535 bytes) , Untitled.png (363 kB)
Hi 各位大侠们
关于press fit的镀铜孔,是否有相关IP标准定义其roughness应该根据不同的孔径,定义为多少合适? 
Roughness是如何测量的? 
现有一客户定义为30um,是否合适?
一般的PCB板厂是否有能力做到这样的要求?


请高手们帮忙解答!

Thanks!
BR/Eileen

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2