TECHNET Archives

July 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 3 Jul 2012 09:04:41 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (276 lines)
Yes. It should be application dependent. No, design layout alone are not sufficient.  For example, mcm with split ground under one Device, if you specify 50%allowable voids, if majority under digital ground, you might see things a bit funny.  If majority voiding under analog, you risk loss ground or over heat burnout.  Qfn by design normally is intend to sink heat from ground.  If you see the via array under the ground plane as per component vendor recommended layout, where are the voids location and size need to be take extra cautions.  Design is not the only one need to pay attention. My 1.9 cents.
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Frank Kriesch [mailto:[log in to unmask]]
Sent: Tuesday, July 03, 2012 03:16 AM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] Antwort: Re: [TN] I'm back and have a question about QFN voids

in my opion,
IPC 610 says, the acceptable amount of voids depends on the application 
and has to be agreed between user and supplier. What counts is the 
contacted area, not the amount of voids. The minimum contactarea may be 
calculated while designing the pwb.

Regards,

Frank



Von:    Phil Bavaro <[log in to unmask]>
An:     <[log in to unmask]>
Datum:  03.07.2012 00:59
Betreff:        Re: [TN] I'm back and have a question about QFN voids
Gesendet von:   TechNet <[log in to unmask]>



Ed,

Welcome back!  I know the feeling.

I have seen high volume production requiring J-STD-001 Class 2 with as 
much as 40 percent voiding survive just fine but I have also experienced 
Class 3 military assemblies which claimed to require less than 10 percent 
voiding.  If you say you need less than 10% then that is your requirement. 
 

Currently I have QFNs on Class 3 assemblies which have all the vias under 
the part belly filled with epoxy and cap plated over which naturally 
reduces the voiding.  There is some debate as to what paste pattern 
optimizes the lack of voids, and I have experimented with all kinds of 
paste shapes. 

I believe that wavesoldering a single via will not accomplish what you 
desire and most likely will cause a myriad of other issues that you should 
want to avoid. 

Here is another approach that you might consider:

Pretin the device so that the belly already has solid solder available to 
melt.  Print paste in the corners of the belly pad, and place and reflow. 
The trick is to not apply too much solder during pretinning as to cause 
misalignment in reflow.  Voiding is initiated at the location of the 
printed paste so minimizing the print area leads to minimizing void 
potential.  Eliminating voids is always a controversial subject so you 
picked a good one to enter back into the forum with.

My $.02 worth.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, July 02, 2012 3:22 PM
To: [log in to unmask]
Subject: Re: [TN] I'm back and have a question about QFN voids

The 25% max void criteria applies to BGAs. I don't think there is any 
hard/fast requirement for voids in QFN devices, but I'm not sure. However, 
your QFN may not work properly if you have even 10% voiding in some cases. 
It depends on the component requirements and the design. You may need <10% 
max loss of solder connection between the belly pad and the matching pad 
on the PWB in order to provide the required thermal transfer or to provide 
sufficient electrical connection (or both!). 
________________________________________
From: TechNet [[log in to unmask]] On Behalf Of grandrien 
[[log in to unmask]]
Sent: Monday, July 02, 2012 4:12 PM
To: [log in to unmask]
Subject: Re: [TN] I'm back and have a question about QFN voids

That is rigth, vacuum is an option, except if you have quite high volume 
production ?
Nevertheless are you sure a max of 25% void is really necessary?


========================================
Message du 02/07/12 13:18
De : "Braddock, Iain (UK)"
A : [log in to unmask]
Copie à :
Objet : Re: [TN] I'm back and have a question about QFN voids

Absolutely......problem solved!

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tan Geok Ang
Sent: 02 July 2012 03:27
To: [log in to unmask]
Subject: Re: [TN] I'm back and have a question about QFN voids

*** WARNING ***
This mail has originated outside your organization, either from an 
external partner or the Global Internet.
Keep this in mind if you answer this message.



Easiest way....Vapour Phase with vacuum?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of grandrien
Sent: Saturday, 30 June 2012 4:51 PM
To: [log in to unmask]
Subject: Re: [TN] I'm back and have a question about QFN voids

Hi ed,

Is your solution to solder the central pad through a PTH on soldeing wave 
?
It seems me very tricky process.

Why not using
- preform
- or distributed vias through the central pad to allow the flux outgasing. 
In that case to avoid the overflow of solder through the vias on the 
opposite PCB side, printed paste around vias, not on them, and add solder 
mask rings around the vias to contain the solder. out of the vias.

QUESTION: requirements on void max are quite always often between 20-30%. 
But looking at thermal studies from different actors such as component 
manufacturers or even OEM or CEM it seems in very most cases the thermal 
impact keeps quite negligeable up to 70-80% and sometime more.
So why everyone keeps the 20-30% requirement ?
Or some of you accept  higher void levels under QFN ?

========================================
Message du 29/06/12 19:04
De : "Ed Popeielarski"
A : [log in to unmask]
Copie à :
Objet : [TN] I'm back and have a question about QFN voids

Greetings 'netters,

For the past 2 1/2 years I've been lurking because Technet didn't get 
along with my employer's email system (specifically during maintenance).

I solved that problem by finding another employer! See how much you guys 
mean to me?!

It's good to be "back in the saddle again", so please allow me to begin 
with a perplexing question:

I need to solve QFN ground-pad voiding on a 0.038" thick ENIG assembly. 
The application is a high power RF amp and voiding as low as 25% causes 
issues with reliability.

Many attempts to resolve this with stencil variations, (thickness, star 
patterns, etc) and process variables (reflow time/temps) have been 
fruitless.

I'm considering re-spinning the board with a via dead center of this 6mm 
part, print & reflow only the leads, then wave solder the via (SAC305 with 
water soluble flux) in hopes of forcing the volatiles out from the center 
due to the wetting forces. Has anyone tried and succeeded with this method 
or am I sailing off the edge of the planet?

Thanks for your help in advance.


Ed Popielarski
Engineering Manager

Technical Services, Inc.
970 NE 21st Ct.
Oak Harbor, Wa. 98277

Ph: 360-675-1322
Fx: 206-624-0965
Cl: 949-581-6601

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


___________________________________________________________
Obligatoire au 1er juillet, achetez votre éthylotest sur Voila.fr 
http://shopping.voila.fr/thematique/ethylotest

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

********************************************************************
This email and any attachments are confidential to the intended recipient 
and may also be privileged. If you are not the intended recipient please 
delete it from your system and notify the sender. You should not copy it 
or use it for any purpose nor disclose or distribute its contents to any 
other person.

MBDA UK Limited, a company registered in England and Wales, registration 
number 3144919 whose registered office is at Six Hills Way, Stevenage, 
Hertfordshire, SG1 2DA, England.

********************************************************************


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


___________________________________________________________
Obligatoire au 1er juillet, achetez votre éthylotest sur Voila.fr 
http://shopping.voila.fr/thematique/ethylotest

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee 
and may contain L-3 proprietary information that may also be defined as 
USG export controlled technical data. If you are not the intended 
recipient, any disclosure, use or distribution of its content is 
prohibited. Please notify the sender by reply e-mail and immediately 
delete this message and any attachments.




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



.
Der Inhalt dieser E-Mail ist für den Absender rechtlich nicht verbindlich.
Informieren Sie uns bitte, wenn Sie diese E-Mail fälschlicherweise erhalten haben (Fax: +49-7551-891-4001). Bitte löschen Sie in diesem Fall die Nachricht. Jede Form der weiteren Benutzung ist untersagt.
.
The content of this e-mail is not legally binding upon the sender.
If this e-mail was transmitted to you by error, then please inform us accordingly (Fax: +49-7551-891-4001). In such case you are requested to erase the message. Any use of such e-mail message is strictly prohibited.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2