TECHNET Archives

July 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Grossmann, Guenter" <[log in to unmask]>
Date:
Fri, 6 Jul 2012 12:18:44 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
<005d01cd5b93$042fe420$0c8fac60$@com>
Subject:
From:
Steve Gregory <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (171 lines)
Hi Günter!

Got your pictures posted, they're here:

http://stevezeva.homestead.com/Dendrite_1.jpg

http://stevezeva.homestead.com/Dendrite_2.jpg

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Grossmann, Guenter
Sent: Friday, July 06, 2012 12:03 PM
To: [log in to unmask]
Subject: [TN] AW: [TN] Copper Dendrites

I sent the to Steve.

Cheers

Günter 


>-----Ursprüngliche Nachricht-----
>Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Victor Hernandez
>Gesendet: Freitag, 6. Juli 2012 17:55
>An: [log in to unmask]
>Betreff: Re: [TN] Copper Dendrites
>
>What happened to the pictures?
>
>Victor,
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Reid
>Sent: Friday, July 06, 2012 10:33 AM
>To: [log in to unmask]
>Subject: Re: [TN] Copper Dendrites
>
>Ah, Now I understand.
>
>Conductive filaments can grow particularly conductive anodic filaments.
>I was thinking of a dendrite of copper not conductive filaments. I 
>expect dendrites to be larger and of pure copper but you may get 
>dendritic growth with a contaminate, in the presents of water and with 
>an electrical potential.
>
>Sorry for my misunderstanding.
>
>Sincerely,
>
>
>
>Paul Reid
>
>Program Coordinator
>
>PWB Interconnect Solutions Inc.
>235 Stafford Rd., West, Unit 103
>Nepean, Ontario Canada, K2H 9C1
>
>613 596 4244 ext. 229
>
>Skype paul_reid_pwb
>[log in to unmask]
>
>
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
>Sent: July 6, 2012 9:23 AM
>To: [log in to unmask]
>Subject: Re: [TN] Copper Dendrites
>
>I agree. I have seen dendrites grow under solder mask from on conductor 
>to another, and from a PTH to a conductor, under solder mask.
>
>If the residue were benign, until exposed to water, and the coating 
>were to protect it from exposure, it could help.
>
>Still, I am skeptical, that it would reduce risk of failure. It would 
>need to be a designed process, not a band aid.
>
>It might make things worse.
>
>Guy
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
>Sent: Friday, July 06, 2012 8:23 AM
>To: [log in to unmask]
>Subject: Re: [TN] Copper Dendrites
>
>Hi Neil
>
>I stand by my earlier posting on this. Neither a solder resist nor a 
>conformal coating will PREVENT dendrites, they might delay it for a 
>while, but then what is lurking and festering underneath..just when you 
>thought it was safe to go back in the water!?
>
>Graham Naisbitt
>
>
>On 5 Jul 2012, at 19:50, Neil Atkinson wrote:
>
>> Thanks everyone for comments so far - haven't been on Technet for a
>while
>so it was good to get such good responses.
>>
>> Really miss Werner for questions like this...
>>
>> Actually we have never seen a failure for dendrites; however, we have
>a
>customer who has a past problem with another supplier due to dendrites 
>on PCBs and as a result wants us to cover vias with solder resist or 
>conformal coating.
>>
>> Tha,
>>
>> Neil
>>
>> _____________________________________________________________________
>> _ This email has been scanned by the Symantec Email Security.cloud
>service.
>> For more information please contact helpdesk at x2960 or 
>> [log in to unmask] 
>> _____________________________________________________________________
>> _
>
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud 
>service.
>For more information please contact helpdesk at x2960 or 
>[log in to unmask] 
>______________________________________________________________________
>
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud 
>service.
>For more information please contact helpdesk at x2960 or 
>[log in to unmask] 
>______________________________________________________________________
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud 
>service.
>For more information please contact helpdesk at x2960 or 
>[log in to unmask] 
>______________________________________________________________________
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud 
>service.
>For more information please contact helpdesk at x2960 or 
>[log in to unmask] 
>______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2