Thanks everyone for comments so far - haven't been on Technet for a
while so it was good to get such good responses.
Really miss Werner for questions like this...
Actually we have never seen a failure for dendrites; however, we have a
customer who has a past problem with another supplier due to dendrites
on PCBs and as a result wants us to cover vias with solder resist or
conformal coating.
Tha,
Neil