TECHNET Archives

July 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Joyce Koo <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 20 Jul 2012 08:47:46 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (154 lines)
Yes, but above 5 Ghz we are talking ultra hi freq.
________________________________________
From: Joyce Koo [[log in to unmask]]
Sent: Friday, July 20, 2012 8:32 AM
To: Stadem, Richard D.; TechNet E-Mail Forum
Subject: RE: [TN] Low Loss PCB Material

You never know if he is talking about 5 or 40 or even automotive radar that could be 24 or 77.

Joyce Koo
Materials Researcher - Materials Interconnect Lab
Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760


-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Friday, July 20, 2012 9:29 AM
To: TechNet E-Mail Forum; Joyce Koo
Subject: RE: [TN] Low Loss PCB Material

High frequency RF is considered to be above 1 ghz, generally speaking. Not sure if this is formalized somewhere?
________________________________________
From: TechNet [[log in to unmask]] On Behalf Of Joyce Koo [[log in to unmask]]
Sent: Friday, July 20, 2012 8:02 AM
To: [log in to unmask]
Subject: Re: [TN] Low Loss PCB Material

How high is "high"?

Joyce Koo
Materials Researcher - Materials Interconnect Lab
Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Friday, July 20, 2012 12:50 AM
To: [log in to unmask]
Subject: Re: [TN] Low Loss PCB Material

Hi Richard,

Thanks a lot.  I will check out these materials.


Regards
Ravinder Ajmani
HGST, a Western Digital company
[log in to unmask]


5601 Great Oaks Pkwy.
San Jose, CA 95119-1003
www.hgst.com




"Stadem, Richard D." <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
07/19/2012 06:54 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D."    <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
Re: [TN] Low Loss PCB Material






Hi, Ravinder
You might want to look at the following:
Nelco N4000-13EP
Panasonic Megtron Getek
Taconic RF-35TC or RF35A2

I know these are all RF-tailored, but not sure if all are halogen free. I
know the Taconic materials are.
You would need to check with them about the UL approval rating.

________________________________________
From: TechNet [[log in to unmask]] On Behalf Of [log in to unmask]
[[log in to unmask]]
Sent: Thursday, July 19, 2012 8:10 PM
To: [log in to unmask]
Subject: [TN] Low Loss PCB Material

Hi All,

We discussed with our quick-turn fab the use of low-loss PCB materials for
high-speed applications.  As per the discussions,the only such material
that is Halogen-Free and has UL Approval seems to be Rogers Theta
material.  If there are other materials available in US and more
importantly at the high-volume fabs off-shore then please share the
information.  I will really appreciate it.

Thanks.


Regards
Ravinder Ajmani
HGST, a Western Digital company
[log in to unmask]


5601 Great Oaks Pkwy.
San Jose, CA 95119-1003
www.hgst.com


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2