Hi Steve,
Usually it used for tape and reels (max temp allowed is 40 degC) so the
temp to be used is 40 degC and level of vacuum level is -25 / -30 inch Hg.
Reuven
On Fri, Jun 1, 2012 at 8:45 PM, Steven Creswick
<[log in to unmask]>wrote:
> Reuven,
>
> Thanks for the approximation. This is without heat - correct? What level
> of vacuum?
>
> Ditto on the radiation and conduction! Absolutely correct!
>
> Steve
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Reuven Rokah
> Sent: Friday, June 01, 2012 1:37 PM
> To: [log in to unmask]
> Subject: Re: [TN] Vacuum Drying of PCB's
>
> Hi Richard,
>
> it about 30% faster and you should know that only thermal radiation and
> thermal conduction work in vacuum oven, no convection because of no air
> exist. You should add more shelves and spread the PCBs / components on the
> shelves to assure good contact.
>
> The advantage is less oxidation on pads / metal parts.
>
> Reuven
>
> On Fri, Jun 1, 2012 at 5:47 PM, Richard Kraszewski <
> [log in to unmask]> wrote:
>
> > I would appreciate anyone sharing their thoughts on vacuum drying of
> PCB's.
> >
> > What conditions do you use? (Time, temp and vacuum)
> >
> > I realize it can be used to reduce required peak temperature but is
> > there potentially any time reduction benefit to using vacuum?
> >
> > I saw a paper from the "Electronic Components and Systems Division
> > within German Electrical and Electronic Manufacturers´Association
> > Working Group", entitled
> >
> > "Recommendation & Guideline Values for drying for bare PCBs"
> >
> > The offered a rather paltry reduction in drying time of 60 minutes
> > from 8 hours if vacuum was used. Doesn't seem like much of a benefit.
> >
> >
> > Rich Kraszewski/PLEXUS
> >
> >
> > ______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud service.
> > For more information please contact helpdesk at x2960 or
> > [log in to unmask]
> > ______________________________________________________________________
> >
>
>
>
> --
>
> Best Regards,
>
> *Reuven Rokah*
>
> Mobile: 972-52-6012018
> Tel: 972-3-9360688
> Fax: 076-5100674
> <http://www.rokah-technologies.com/>[log in to unmask]
> [log in to unmask]
> www.rokah-technologies.com
>
> **
> This e-mail message is intended for the recipient only and contains
> information which is CONFIDENTIAL and which may be proprietary of Rokah
> Technologies. If you have received this transmission in error, please
> inform
> me by e-mail, phone or fax, and then please delete all of the original
> files
> and all other copies exist.
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
--
Best Regards,
*Reuven Rokah*
Mobile: 972-52-6012018
Tel: 972-3-9360688
Fax: 076-5100674
<http://www.rokah-technologies.com/>[log in to unmask]
[log in to unmask]
www.rokah-technologies.com
**
This e-mail message is intended for the recipient only and contains
information which is CONFIDENTIAL and which may be proprietary of Rokah
Technologies. If you have received this transmission in error, please
inform me by e-mail, phone or fax, and then please delete all of the
original files and all other copies exist.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|