Could I have also a copy. Thanks.
Grandrien.
========================================
Message du 27/06/12 17:08
De : "Amol Kane (Asteelflash,US)"
A : [log in to unmask]
Copie à :
Objet : Re: [TN] Chemtronics Konform SR Conformal Coating
I would be very interested to see it. Thank you Louis!!
Regards,
Amol
-----Original Message-----
From: Louis Hart [mailto:[log in to unmask]]
Sent: Wednesday, June 27, 2012 10:29 AM
To: TechNet E-Mail Forum; Amol Kane (Asteelflash,US)
Subject: RE: Chemtronics Konform SR Conformal Coating
Amol, If you want, have a look at a short technical paper I put in the
August 2002 IPC Review, describing the experimentation done to set up
an automated conformal coater. Summer of 2010 that authority Doug Pauls
looked at it and did not recommend putting it in the trash, so it may
have some worthwhile ideas. The website IPC archives for that
publication do not go back to 2002. Let me know if you want to see it
and I will dig up a copy. Louis Hart
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
(Asteelflash,US)
Sent: Wednesday, June 27, 2012 7:55 AM
To: [log in to unmask]
Subject: [TN] Chemtronics Konform SR Conformal Coating
Dear Technetters,
I am being tasked to setup the above coating with the PVA automatic
spray/dispense machine (fine spray head and the needle dispense head).
The coating comes in two forms, the Konform SR and Konform SR High
viscosity, and some mixing is involved to arrive at the optimal
viscosity. I plan to talk to PVA and get their expertise in setting up
the machine and eventually setting up a DOE to determine the optimal
viscosity specification limits. However I wanted to know if there are
any techentters already spraying this coating thru automated conformal
coating equipment. I was hoping to talk to someone who is willing to
share his/her experience with this coating and hopefully obtain
information on some "good" starting values
Thanks,
Amol
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
___________________________________________________________
Obligatoire au 1er juillet, achetez votre éthylotest sur Voila.fr http://shopping.voila.fr/thematique/ethylotest
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|