Richard,
Look at ARP 1332 Rev C section 6.2.2. You should find the answer you want there. ARP1332 is published and Copyrighted by SAE and you can obtain a copy from them with the following contact info:
TO PLACE A DOCUMENT ORDER: Tel: 877-606-7323 (inside USA and Canada)
Tel: 724-776-4970 (outside USA)
Fax: 724-776-0790
Email: [log in to unmask]
SAE WEB ADDRESS: http://www.sae.org
Regards,
Thomas A. Carroll, CQA, CIT, FAA ODA Unit Member
Supplier Quality Engineer
Boeing Defense, Space and Security - East Region Supplier Quality
eFAX: 314-777-1845
Cell: 215-692-2463
Virtual Desk Phone Number: 314-545-2358
email: [log in to unmask]
Go Green! Please do not print this e-mail unless necessary.
NOTE: This communication may contain privileged or other confidential information. If you are not the intended recipient, or believe you have received this communication in error, please do not print, copy, retransmit, disseminate, or otherwise use the information. Also, please indicate to the sender that you have received this e-mail in error, and delete the copy you received. Thank you.
EXPORT COMPLIANCE STATEMENT:
"The information contained herein is or may be controlled by the International Traffic in Arms Regulations (ITAR), 22 CFR 120-130, and may not be exported, or disclosed to a foreign person, whether in the United States or abroad, without prior U.S. Government written approval"
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Wednesday, May 23, 2012 6:28 PM
To: [log in to unmask]
Subject: [TN] Spot test for Rosin Residue
I seem to recall a wet chemical spot test for rosin residues.
Something that required:
* Piece of filter paper.
* Sugar solution .
* Dilute Sulfuric acid.
If the final spot went red, it would indicate the presence of rosin.
Does anybody recall this test and have the details?
Thanks in advance
Rich Kraszewski
Plexus Engineering Solutions
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|