Hence my "all other things being equal" statement.
Dewey
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, May 16, 2012 11:28 AM
To: TechNet E-Mail Forum; Whittaker, Dewey (EHCOE)
Subject: RE: [TN] Through hole barrel voids
Let me state the obvious even though I did not see it mentioned.....it
is possible to double side hand solder and trap large voids in the
barrel.....I know because I have seen an engineer attempt this. In his
mind, the solder joints looked great and visually it was
compliant.....but I advised him that the procedure was not authorized
and proceeded to xray the connection and show him the error in his ways.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Wednesday, May 16, 2012 10:45 AM
To: [log in to unmask]
Subject: Re: [TN] Through hole barrel voids
To reject, or not to reject, that is the question:
Whether 'tis Nobler in the mind to suffer The Slings and Arrows of
unfortunate outgassing, Or to take X-rays against a Sea of voids, And by
opposing accept them: to die, to pry No more; and say we end the
heart-ache, and the thousand thermal shocks That the assembly is heir
to? 'Tis a consummation Devoutly to be wished for those who don't have a
bodkin against their chest to honor the bottom line.
Barring the chance that I have missed the connection and this was a
metaphorical response to voids or unfulfilled expectations in life and
not the printed board assembly: all other things being equal; I would
accept them (the PTH voids) as-is.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eva J
Sent: Wednesday, May 16, 2012 9:37 AM
To: [log in to unmask]
Subject: Re: [TN] Through hole barrel voids
Craig,
Was this PCB/ connector subjected to wave solder, hand solder and or
intrusive pin/paste solder process?
I have seen touch up soldering to " fill the barrel" on the component
side create voids and contaminant entrapment which may be a reliability
issue.
What is the cumulative fill? Solder fill provides the mechanical
strength to withstand its service environment.
Eva
Spec Tech
On Wed, May 16, 2012 at 9:12 AM, David D. Hillman <
[log in to unmask]> wrote:
> Hi Craig! One of the downsides of now having access to Xray inspection
> technology is that we can see many "things" we never could before -
> which now causes the question "is that bad?". There is currently no
> plated thru hole void criteria in the IPC JSTD 001 specification. I
> would recommend that an assessment of the assembly be initiated.
> Pulling and inspecting a number of assemblies that either have been in
> the field or have passed all of the qualification tests will
> demonstrate what level of voids typically exist and if that level of
> voiding is a reliability issue. The presence of voids is not
necessarily an indication of a reliability issue. Good Luck.
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
>
>
> Craig Sullivan <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
> 05/16/2012 07:14 AM
> Please respond to
> TechNet E-Mail Forum <[log in to unmask]>; Please respond to Craig
> Sullivan <[log in to unmask]>
>
>
> To
> <[log in to unmask]>
> cc
>
> Subject
> [TN] Through hole barrel voids
>
>
>
>
>
>
> Hi everyone,
>
>
>
> We have a certain board with several through hole connectors. The
> customer has provided us x ray images showing voiding in the barrels.
> Fillets on both sides are acceptable, and the solderability tests are
> ok. This seems to be isolated to this board because random sampling on
> other boards shows virtually no voiding. The only voiding "criteria" I
> can find is related to BGAs. Is there any published criteria /
> reference material for this type of defect?
>
>
>
> Thank you,
>
> Craig Sullivan
>
> Manufacturing Engineer
>
> MPL Incorporated
>
> P: 607.266.0480
>
> F: 607.266.0482
>
> <mailto:[log in to unmask]> [log in to unmask]
>
> P Please consider the environment before printing this e-mail.
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|