Joyce,
My apology. I read the posting too quickly. I the question was about electroless nickel and now I realize it was electrolytic which doesn't have P.
Regards,
George
George M. Wenger
Senior Principal Reliability / FMA Engineer
Andrew Corporation - Wireless Network Solutions
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 Office (732) 309-8964 Mobile
E-mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Tuesday, May 29, 2012 1:14 PM
To: [log in to unmask]
Subject: Re: [TN] Phosphorus at the BGA pad
No. I think. I'll wait for someone to correct me if I am wrong.
Joyce Koo
Materials Researcher - Materials Interconnect Lab Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Ayotte
Sent: Tuesday, May 29, 2012 12:55 PM
To: [log in to unmask]
Subject: [TN] Phosphorus at the BGA pad
There has been some discussion recently on the phosphorus level for ENiG.
My question is:
- for electrolytic nickel and gold deposition
- would you expect to find phosphorus at the soldered interface?
Thanks.
Stephen Ayotte
Manufacturing Quality Engineer
Bldg. 966 - 2, Office 2J1309
Userid: Stephen Ayotte/Burlington/IBM
Internet id: [log in to unmask]
Phone: 802 769 4775
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|